Ah yes, apologies, I misread the first post thinking this was using a vinyl ester tooling gelcoat.
I agree with Mark, the epoxy tooling system is extremely viscous and you need to be very meticulous about the way you apply the gelcoat. You will find the Unimould system is somewhat more forgiving.