Nusse
Nusse
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 50
Hi all,
This is my very first post...
I'm thinking of buying an autoclave. I have only received a few pictures so far.
It's 2 meter long and 0.9 m i diameter (inside). It's probably only approved for 3 bar.
50 years old and used for vacuum and steam threatment at a yarn factory, I think...
I will probably have to redo a lot to make it work.
Price: ~£500. What do you think.
PS I have no experience of prepreg and autoclave so far ;-)
Best Regards,
Magnus
Attachments
koenig.jpg
(
2 views,
672.00 KB
)
Reply
Like
3
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
What are you making? In my opinion, OOA pre-preg makes autoclaves pretty redundant unless you're doing stuff for the F1.
Reply
Like
3
scottracing
scottracing
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
As hanaldo says ooa pre pregs are just as good depending on your application.
autoclaves arent cheap to run and you will probably need to do a bit of work to that one to make it suitable.
Reply
Like
3
Nusse
Nusse
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 50
Thanks for your input.
Today I'm not doing any composites work at all. I understand that for most jobs an aotoclave is not at all necessary.
//Magnus
Reply
Like
3
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
I'd give it a miss then. Build yourself a simple oven with a good PID controller and get into OOA pre-pregs. It's great stuff, exceptionally easy to use and you won't waste the time and money you would trying to repurpose that autoclave.
Reply
Like
3
scottracing
scottracing
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
I managed to purchase a couple of laboratory ovens of ebay and with a decent vac pump its great for curing composites.
Have a good look on the easy composite you tube videos and through the projects on here, then start pricing up all the materials and consumables you need, its not a cheap hobby
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search