carbon man
carbon man
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 86,
Visits: 1.2K
When applying the gloss pva release agent it always drys with tiny air bubbles in which are raised up and show up in the new mould, then I'm forever sanding the new mould.
Iv tried using a foam bush, iv tried wiping on with tissue, and iv tried using a small air spray gun that attaches to a little air canister. But I found when spraying the pva on it sometimes beaded which wad also no good.
Hope you can help.
Cheers
Reply
Like
3
carbonfibreworks
carbonfibreworks
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
Hi Carbon Man
Thoroughly de grease the part then use a spray gun and build the PVA up with some light mist coats , I am not a fan of PVA it has its applications .
Chris
Reply
Like
3
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
You did too heavy a coat. Have had this issue before as well. You need to apply it a bit thinner, and allow it to completely dry between coats. Also make sure it isn't too hot when you are spraying.
Reply
Like
3
carbon man
carbon man
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Awaiting Activation
Posts: 86,
Visits: 1.2K
Thanks for the reply. Iv read up about using hairspray! I tried this method and wow! Perfect results!
Reply
Like
2
Blackrat
Blackrat
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 20,
Visits: 85
hairspray and PVA ? please do tell ....
Reply
Like
3
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Hairspray does the same thing as PVA, so it can be used instead of. It's more expensive though, so seems a bit pointless to me unless you're in a grind.
Reply
Like
2
carbon man
carbon man
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Awaiting Activation
Posts: 86,
Visits: 1.2K
Yeah used instead of pva. As I didn't have a great spray gun. And all my parts are small so cost of hairspray isn't a problem. New mould is like glass
Reply
Like
2
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Nice. Always good when things work out. Photos? I enjoy a nice glossy mould
Reply
Like
3
fastboats
fastboats
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 9,
Visits: 94
Nice hairspray trick. How many layers did you use and any other tricks you can tell on using it vs. Pva?
Thanks
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search