Nice hairspray trick. How many layers did you use and any other tricks you can tell on using it vs. Pva?

Thanks
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Nice. Always good when things work out. Photos? I enjoy a nice glossy mould BigGrin
carbon man
carbon man
Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
Yeah used instead of pva. As I didn't have a great spray gun. And all my parts are small so cost of hairspray isn't a problem. New mould is like glass Smile 
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Hairspray does the same thing as PVA, so it can be used instead of. It's more expensive though, so seems a bit pointless to me unless you're in a grind. 
Blackrat
Blackrat
Supreme Being (148 reputation)Supreme Being (148 reputation)Supreme Being (148 reputation)Supreme Being (148 reputation)Supreme Being (148 reputation)Supreme Being (148 reputation)Supreme Being (148 reputation)Supreme Being (148 reputation)Supreme Being (148 reputation)
Group: Forum Members
Posts: 20, Visits: 85
hairspray and PVA ? please do tell ....
carbon man
carbon man
Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
Thanks for the reply. Iv read up about using  hairspray! I tried this method and wow! Perfect results!
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You did too heavy a coat. Have had this issue before as well. You need to apply it a bit thinner, and allow it to completely dry between coats. Also make sure it isn't too hot when you are spraying. 
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi Carbon Man 
Thoroughly de grease the part then use a spray gun and build the PVA up with some light mist coats , I am not a fan of PVA it has its applications .
Chris

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
carbon man
carbon man
Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)Supreme Being (760 reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
When applying the gloss pva release agent it always drys with tiny air bubbles in which are raised up and show up in the new mould, then I'm forever sanding the new mould. 

Iv tried using a foam bush, iv tried wiping on with tissue, and iv tried using a small air spray gun that attaches to a little air canister. But I found when spraying the pva on it sometimes beaded which wad also no good.

Hope you can help. 

Cheers 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search