This is a replacement carbon end cap we have recently made for new Fireblade raced by Sam Boyers, made from pre preg carbon..
Chris
Carbon fibre works
Training and manufacture







http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Edited 11 Years Ago by carbonfibreworks
Dravis
Dravis
Supreme Being (8.8K reputation)Supreme Being (8.8K reputation)Supreme Being (8.8K reputation)Supreme Being (8.8K reputation)Supreme Being (8.8K reputation)Supreme Being (8.8K reputation)Supreme Being (8.8K reputation)Supreme Being (8.8K reputation)Supreme Being (8.8K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Very nice -- I can not tell that from the factory one .. did the original melt ?Cool

That rear tyre looks "well used" ..  w00t

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
carbonfibreworks
carbonfibreworks
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi Dravis
He fell off and damaged the original cap, the rider is Sam Boyers and he is very quick and normally keeps on the black but he must have been having a bad daySmile
Regards Chris

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search