Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Motorsport, Vehicle Design and Modification
»
Carbon end can
Carbon end can
Post Reply
Like
5
Carbon end can
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
carbonfibreworks
carbonfibreworks
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
Hi Dravis
He fell off and damaged the original cap, the rider is Sam Boyers and he is very quick and normally keeps on the black but he must have been having a bad day
Regards Chris
Reply
Like
7
Dravis
Dravis
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 592,
Visits: 1.9K
Very nice -- I can not tell that from the factory one .. did the original melt ?
That rear tyre looks "well used" ..
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
Reply
Like
7
carbonfibreworks
carbonfibreworks
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
This is a replacement carbon end cap we have recently made for new Fireblade raced by Sam Boyers, made from pre preg carbon..
Chris
Carbon fibre works
Training and manufacture
Edited
11 Years Ago by
carbonfibreworks
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search