8/27/2015 8:11:06 PM
This is a replacement carbon end cap we have recently made for new Fireblade raced by Sam Boyers, made from pre preg carbon..
Chris
Carbon fibre works
Training and manufacture
By carbonfibreworks
-
8/28/2015 7:53:09 PM
Hi Dravis
He fell off and damaged the original cap, the rider is Sam Boyers and he is very quick and normally keeps on the black but he must have been having a bad day