Print throu epoxy


Author
Message
thanasiss3
thanasiss3
Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)Supreme Being (116 reputation)
Group: Forum Members
Posts: 18, Visits: 348
Hi,i make carbon fibre laminates and have the following issues at some parts which get direct sunlight in the hot interior of a car

I 'post cure'the parts for some hours at 40celcius under the sun,but it seem the interior get hotter
Do i need higher temp post cure to avoid it?

This is the part after buffing the clear coat







http://i1293.photobucket.com/albums/b586/mad8shanasiss3/received_10206473749783589_zpsd81opsvx.jpeg

This after the paint through







http://i1293.photobucket.com/albums/b586/mad8shanasiss3/IMG_20150627_143652_zpsxamjqf12.jpg
Edited 10 Years Ago by thanasiss3
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You need to let it cool down again yes. 

This may take a bit of experimentation without the TDS, as it's possible that 75 is just too far above your resins Tg and it could be degrading the resin. Don't forget a nice yet though, you need to let the part cool back down to ambient temperature before you debag. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
thanasiss3 - 10 Years Ago
Hanaldo - 10 Years Ago
thanasiss3 - 10 Years Ago
Hanaldo - 10 Years Ago
thanasiss3 - 10 Years Ago
Dravis - 10 Years Ago
thanasiss3 - 10 Years Ago
Hanaldo - 10 Years Ago
thanasiss3 - 10 Years Ago
Hanaldo - 10 Years Ago
thanasiss3 - 10 Years Ago
Warren (Staff) - 10 Years Ago
thanasiss3 - 10 Years Ago
Warren (Staff) - 10 Years Ago