andelise
andelise
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 81
hi guys.
so after it comes out of the mould how do we bring it to a shine, g10 and pad or dose it come out with a shine?
thanks guys
Reply
Like
3
baja_patient
baja_patient
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 135,
Visits: 1.6K
In theory, the surface of your part will have exactly the same shine/texture that your mould surface has. Thus the shinier your mould, the shinier the part will be. If your mould is not quite as shiny as you would like, wet sand through all the grits starting at 240-400 up to 2000, then use polishing compounds.
Alternatively, if the finish is smooth, but matt, then hit it with an automotive clear coat. That is what I do, it comes out very glossy. Automotive clear can also be polished nicely.
hope it helps,
cheers
Reply
Like
2
andelise
andelise
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 81
thanks mate very helpful. iv made 2 moulds today and not
happy with the shine yet but will wet sand now
andy
Reply
Like
3
baja_patient
baja_patient
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 135,
Visits: 1.6K
No probs mate, after reading my post again i noticed it could cause some confusion. You can wetsand and polish your moulds thats fine.
With the clearcoat I meant the finished part.
Do not clear coat the mould.
good luck with your bits!
cheers
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search