By andelise - 6/3/2012 5:25:28 PM				
            
                      
            hi guys.
  so after it comes out of the mould how do we bring it to a shine, g10 and pad or dose it come out with a shine?
  thanks guys
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By baja_patient - 6/5/2012 12:27:39 PM				
            
                      
            No probs mate, after reading my post again i noticed it could cause some confusion. You can wetsand and polish your moulds thats fine. 
  With the clearcoat I meant the finished part. Do not clear coat the mould. 
  good luck with your bits!
  cheers
           
		 | 			
		 
	
	
						
		 	
		
	 |