Hi guys

I have an idea in mind to make a golf cart using CF. I will use my cart as model but there is some bended parts  that I don't know how to reproduce. I dont have it with me right now and I dont know the exact dimensions but the parts are ab. 1m long, 3-5 cm diameter with a 45 degrees (ish) hinge in the middle.

Any ideas how to make that ? Sould I buy some tubes and connect them with an adhesive? or with some cloth (sleeve ?)? Should I make it all with CF sheets / sleeve?

Cheers from Newcastle !

Pierre
Reply
Pertabolis
Pertabolis
Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)Supreme Being (177 reputation)
Group: Forum Members
Posts: 17, Visits: 193
Thanks all

I understand that is quite difficult to realize.
BTW I was thinking about a bended tube, not a hinge sorry. My english is not really as it should be...

Cheers
Pierre
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search