bended tube


Author
Message
Pertabolis
Pertabolis
Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)
Group: Forum Members
Posts: 17, Visits: 193
Hi guys

I have an idea in mind to make a golf cart using CF. I will use my cart as model but there is some bended parts  that I don't know how to reproduce. I dont have it with me right now and I dont know the exact dimensions but the parts are ab. 1m long, 3-5 cm diameter with a 45 degrees (ish) hinge in the middle.

Any ideas how to make that ? Sould I buy some tubes and connect them with an adhesive? or with some cloth (sleeve ?)? Should I make it all with CF sheets / sleeve?

Cheers from Newcastle !

Pierre
Wabba
Wabba
Supreme Being (325 reputation)Supreme Being (325 reputation)Supreme Being (325 reputation)Supreme Being (325 reputation)Supreme Being (325 reputation)Supreme Being (325 reputation)Supreme Being (325 reputation)Supreme Being (325 reputation)Supreme Being (325 reputation)
Group: Forum Members
Posts: 21, Visits: 64
Hello Pierre,

Take a look at a thread under Recreational and Sports Equipment labeled Inflatable Bladder Mould. It gives some pretty creative options. I can't think of any better advice at least at the moment.

Good luck with your project!
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Pierre,

I dont have it with me right now and I dont know the exact dimensions but the parts are ab. 1m long, 3-5 cm diameter with a 45 degrees (ish) hinge in the middle.


When you say hinge to you mean hinge (i.e. a moving, articulated section) or a rigid bend? - If it's a hinge then I'd probably suggest not making that section out of carbon fibre and using a more appropriate material instead.

If you do mean a bend then this is quite difficult to do in carbon fibre because it requires either a split-mould that's difficult to get inside to lay up or a rigid mandel that's difficult to remove which is why you're left considering inflatable bladders. If you have limited experience of composites at the moment I would probably avoid this particularly difficult problem at first.

Best regards, Matt


Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Edited 14 Years Ago by Matt (Staff)
Pertabolis
Pertabolis
Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)Supreme Being (263 reputation)
Group: Forum Members
Posts: 17, Visits: 193
Thanks all

I understand that is quite difficult to realize.
BTW I was thinking about a bended tube, not a hinge sorry. My english is not really as it should be...

Cheers
Pierre