Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Equipment and Materials
»
Measurement equipment for thickness
Measurement equipment for thickness
Post Reply
Like
3
Measurement equipment for thickness
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
xkotx
xkotx
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 14
Hi all,
I'm looking for some kind of measurement equipment , which will be able to read thickness in few different places(not only edges) of a part. Something what can be used by operator. Thank you.
Reply
Like
3
scottracing
scottracing
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
checking thickness of material? or cured laminates?
a good pair of verniers and a micrometer are usually enough, you get specialised measuring calipers for checking material thickness thats used in the textile industry if you want to measure fabrics.
Reply
Like
2
xkotx
xkotx
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 14
Thank you for your replay.Its for cured part.
For example: Let say that the part is 1,5m long and 1,5m wide and has complicated shape.
I would like to check thickness in the middle and with caliper or micrometer i will not be able to reach those points. Thx
Reply
Like
3
Dravis
Dravis
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 592,
Visits: 1.9K
This can be done using a dial indicator (or "Dial clock" the ones used to indicate runout on a lathe, or movement on a milling machine.)
http://www.rdgtools.co.uk/cgi-bin/sh000001.pl?WD=dial&PN=CLOCKS__DIGITAL___MANUAL.html#a398475
You need to build a stable "rig" in effect a large "U-shaped" metal construction, with an adjustable point on the lower part, and a mounting point for the dial indicator or "dial clock"
This "u" needs to be big/deep enough to allow you to reach the middle of your largest work-piece
You can then set the dial indicator to zero on the adjustable point, and measure away ..
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
Reply
Like
2
xkotx
xkotx
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 14
Thx
Dravis
but I'm looking for something like this:
http://www.omnitron.co.uk/portable-ultrasonic-thickness-tester-gauge-glass-metal-plastic-p-388.html
Something what will not require extra work
and what will be handy for operator. Cheers!
Edited
10 Years Ago by
xkotx
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search