Hi all,
I'm looking for some kind of measurement equipment , which will be able to read  thickness in few different places(not only edges) of a part. Something what can be used by operator.  Thank you.
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
checking thickness of material? or cured laminates?

a good pair of verniers and a micrometer are usually enough, you get specialised measuring calipers for checking material thickness thats used in the textile industry if you want to measure fabrics.
xkotx
xkotx
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 3, Visits: 14
Thank you for your replay.Its for cured part.
For example: Let say that the part is 1,5m long and 1,5m wide and has complicated shape. 
I would like to check thickness in the middle and with caliper or micrometer i will not be able to reach those points. Thx
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
This can be done using a dial indicator (or "Dial clock" the ones used to indicate runout on a lathe, or movement on a milling machine.)
 
http://www.rdgtools.co.uk/cgi-bin/sh000001.pl?WD=dial&PN=CLOCKS__DIGITAL___MANUAL.html#a398475

You need to build a stable "rig"   in effect a large "U-shaped" metal construction, with an adjustable point on the lower part, and a mounting point for the dial indicator or "dial clock" 

This "u" needs to be big/deep enough to allow you to reach the middle of your largest work-piece

You can then set the dial indicator to zero on the adjustable point, and measure away .. BigGrin

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
xkotx
xkotx
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 3, Visits: 14
Thx Dravis but I'm looking for something like this:
http://www.omnitron.co.uk/portable-ultrasonic-thickness-tester-gauge-glass-metal-plastic-p-388.html

Something what will not require extra work Smile and what will be handy for operator. Cheers!
Edited 10 Years Ago by xkotx
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search