Repairing a carbon fibre side skirt


Author
Message
John Rutter
John Rutter
Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)
Group: Forum Members
Posts: 7, Visits: 27
Gents,

Total novice looking for advice. I am a novice car restorer (engine builds etc.) but lacking in bodywork skills. I have been lucky enough to purchase a Lambo with carbon fibre side skirts. They have been damaged by kerbs. I have just been quoted £4000 to have them repaired which seems nonsense.  the damage is low down so I reckon the weave may not match perfectly but as it is dark it should not matter too much. Do you think this could be repaired using one of your kits, and if so which one should I purchase? Regards, John
Attachments
photo 1.JPG (622 views, 710.00 KB)
photo 2.JPG (510 views, 665.00 KB)
Reply
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Errrhmm .. Doze... Its NOT "Fake Carbon"    The skirts are actually Carbon -kevlar items ... Original ones it would seem ... Repairing them with new Carbon is just the natural way to do it.

Nothing "fake" about adding a new extra layer of REAL carbon-fibre .. BigGrin

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
John Rutter - 10 Years Ago
Warren (Staff) - 10 Years Ago
John Rutter - 10 Years Ago
Dravis - 10 Years Ago
John Rutter - 10 Years Ago
Warren (Staff) - 10 Years Ago
Dravis - 10 Years Ago
Hanaldo - 10 Years Ago
FLD - 10 Years Ago
John Rutter - 10 Years Ago
tomzi1234 - 10 Years Ago
Dravis - 10 Years Ago
John Rutter - 10 Years Ago
Dravis - 10 Years Ago
tomzi1234 - 10 Years Ago
John Rutter - 10 Years Ago
scottracing - 10 Years Ago
John Rutter - 10 Years Ago

Similar Topics