Author
Message
John Rutter
John Rutter
Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)
Group: Forum Members
Posts: 7, Visits: 27
Gents,

Total novice looking for advice. I am a novice car restorer (engine builds etc.) but lacking in bodywork skills. I have been lucky enough to purchase a Lambo with carbon fibre side skirts. They have been damaged by kerbs. I have just been quoted £4000 to have them repaired which seems nonsense.  the damage is low down so I reckon the weave may not match perfectly but as it is dark it should not matter too much. Do you think this could be repaired using one of your kits, and if so which one should I purchase? Regards, John
Attachments
photo 1.JPG (591 views, 710.00 KB)
photo 2.JPG (492 views, 665.00 KB)
Reply
John Rutter
John Rutter
Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)Forum Guru (53 reputation)
Group: Forum Members
Posts: 7, Visits: 27
Thanks Dravis, I like the idea of creating a 'feature line away from the damaged area. I will study the help videos and if its OK with you reply if I have any further questions. if it does not look too god I can always paint it afterwards!

Regards,




John
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
John Rutter - 10 Years Ago
Warren (Staff) - 10 Years Ago
John Rutter - 10 Years Ago
Dravis - 10 Years Ago
John Rutter - 10 Years Ago
Warren (Staff) - 10 Years Ago
Dravis - 10 Years Ago
Hanaldo - 10 Years Ago
FLD - 10 Years Ago
John Rutter - 10 Years Ago
tomzi1234 - 10 Years Ago
Dravis - 10 Years Ago
John Rutter - 10 Years Ago
Dravis - 10 Years Ago
tomzi1234 - 10 Years Ago
John Rutter - 10 Years Ago
scottracing - 10 Years Ago
John Rutter - 10 Years Ago