Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Cutting carbon fiber and core panel
Cutting carbon fiber and core panel
Post Reply
Like
9
Cutting carbon fiber and core panel
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Ahmedgehad
Ahmedgehad
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 30
Hello,
I would like to cut through various carbon fiber panels with a range of EasyCell75 foam core (3mm, 10mm, 20mm). Will a dremel cutting tool be adequate for cutting through these panels?
Thank you
Tags
carbon fiber
core
cutting
dremel
easycell75
Reply
Like
9
davro
davro
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 300,
Visits: 2.2K
Hi Ahmedgehad,
The 32mm rotary disc with a dremal cuts like a champ
https://www.easycomposites.co.uk/permagrit-32mm-rotary-disc-with-arbor
Have used mine quite a lot ...
David Stevens
YouTube
: 
Comment | Rate | Subscribe
Instagram
Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale
Edited
11 Years Ago by
davro
Reply
Like
10
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Just keep the carbon dust well away from the electric motor of the dremel!! Have had 4 of them go bang in my hand, never a pleasant sensation.
Reply
Like
9
davro
davro
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 300,
Visits: 2.2K
Yup good advice Hanaldo!
My little cordless Dremal is suffering from living in an atmosphere of carbon dust
Won't be long till I treat myself to decent
https://www.easycomposites.co.uk/tools/Dremel-Fortiflex-9100-Heavy-Duty-Flexshaft-and-Hanging-Motor.aspx?117585
And use a decent quality mask, eye protection, ear protection, gloves, codpeice !
David Stevens
YouTube
: 
Comment | Rate | Subscribe
Instagram
Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale
Edited
11 Years Ago by
davro
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search