Hi guys so I'm still busy making my carbonfiber/kevlar Keeperhelmet 
http://www.talkcomposites.com/1066/Carbon-Fiber-Goalie-helmet-field-hockey?PageIndex=3#bm1562

So I'm planning using vacuum infusion, but without gelcoat...since I had loads of problems with the epoxy gelcoat
So I will do it the same way as EC guys did it with their first tutorial video "How to Do Perfect Vacuum Resin Infusion of a Carbon Fibre (Fiber) Part" I guess well know by all of you here Wink

The plan is to clamp of the vacuumhose at the end so I have some "excess" resin to have a nice finish... Is this a good way of thinking first of all?
So I was thinking...If I would still have Pinholes or airbubbles, could I be able to spraygun some epoxy infusion resin IN-2 onto the part and let it cure with a good finish?

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
thx for sharing that information, sounds like a good idea!

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search