So I will do it the same way as EC guys did it with their first tutorial video "How to Do Perfect Vacuum Resin Infusion of a Carbon Fibre (Fiber) Part" I guess well know by all of you here 
The plan is to clamp of the vacuumhose at the end so I have some "excess" resin to have a nice finish... Is this a good way of thinking first of all?
So I was thinking...If I would still have Pinholes or airbubbles, could I be able to spraygun some epoxy infusion resin IN-2 onto the part and let it cure with a good finish?