tomzi1234
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 40,
Visits: 500
i haven't been doing yet a mate/satin finish.
is there a special release agent for mate/satin finish or just wet-send without polishing?
if only sending which grit 1500 or less ?
thank you for answers
Reply
Like
3
Reply
tomzi1234
tomzi1234
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 40,
Visits: 500
thank you
but is it durable, or first mud will leave marks?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
mate finish
tomzi1234
-
10 Years Ago
Hi You can wet sand with 600 grit paper or slightly finer if desired and use Easylease as your...
carbonfibreworks
-
10 Years Ago
thank you but is it durable, or first mud will leave marks?
tomzi1234
-
10 Years Ago
I have done quite a few parts in "satin finish" by wet sanding to 1000 and then used ordinary wax...
Dravis
-
10 Years Ago
thank you for reply
tomzi1234
-
10 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search