thank you for reply
Edited 10 Years Ago by tomzi1234
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
I have done quite a few parts in "satin finish" by wet sanding to 1000 and then used ordinary wax release... no problems with demoulding...

Normally I just wet sand the part after release for m a polished mould, then polish with coarse compound, and use wax on top..

Seems to be just as durable as any satin clear coat, especially when using GC50 gelcoat ..

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
tomzi1234
tomzi1234
Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)
Group: Forum Members
Posts: 40, Visits: 500
thank you

but is it durable, or first mud will leave marks?
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi
You can wet sand with 600 grit paper or slightly finer if desired and use Easylease as your release agent.
Regards Chris
Carbon fibre works LTD

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
tomzi1234
tomzi1234
Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)Supreme Being (303 reputation)
Group: Forum Members
Posts: 40, Visits: 500
i haven't been doing yet a mate/satin finish.

is there a special release agent for mate/satin finish or just wet-send without polishing?
if only sending which grit 1500 or less ?

thank you for answers Smile