Carbon canoe - pitting and bubbling in gel coat - what is cause and what products needed


Carbon canoe - pitting and bubbling in gel coat - what is cause and what products needed
Author
Message
flash68
flash68
Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)
Group: Forum Members
Posts: 7, Visits: 67
Hi, my wife has a full carbon Allwave Vanguard Outrigger canoe.

It is only about 12 months old and we have just removed the cover after being stored for the winter to find an extensive 'roughness' on the gel coat - like tiny bubbles, really course to the touch. Also in places, there is visible bubbling, see picture.

She has only over used plain water to clean it (after ever use) and 'Car Plan bumper shine' to polish it, which was recommended by the seller.
It has been stored in a nylon sock and not come into contact with any chemicals. There was no problem when it was last used in October/early November - could frost have damaged it?

Firstly, can you suggest what might have caused the problem, and secondly what products do I need to repair it. I specifically want to know if I need to colour the gel coat (the boat has a multi-colour design!!) or will I be able to just sand away the bubbles and re-coat it with clear gel.

http://www.talkcomposites.com/Uploads/Images/72351c7a-f577-4d35-8090-1824.jpg
(The darker lines are reflection of trees)
Replies
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi 
This does not answer your question but as its only 12 months old I would be contacting the manufacturer.
Regards Chris
Carbon fibre works LTD

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
flash68
flash68
Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)
Group: Forum Members
Posts: 7, Visits: 67
Hi Chris,
Unfortunately, it was bought second hand so the warranty does not extend to us.
And in any case I now think it is due to the salt water in the bulkhead - fault of the previous owner and our lack of knowledge in not checking and leaving it.
We would be interested in finding someone who can do this repair. I've done my share of car body repair but Im daunted by this because of how thin the gelcoat is.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
flash68 - 10 Years Ago
panda - 10 Years Ago
flash68 - 10 Years Ago
Warren (Staff) - 10 Years Ago
ChrisR - 10 Years Ago
flash68 - 10 Years Ago
dbcrx - 10 Years Ago
flash68 - 10 Years Ago
carbonfibreworks - 10 Years Ago
flash68 - 10 Years Ago
dbcrx - 10 Years Ago
Dravis - 10 Years Ago
flash68 - 10 Years Ago
panda - 10 Years Ago
flash68 - 10 Years Ago