pre preg curing temps?


Author
Message
Toffee
Toffee
Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)
Group: Forum Members
Posts: 36, Visits: 118
hi guys, I would like to hear at what temperatures you guys cure your pre preg parts at? I have an oven which I can get up to 70 degrees quite easily, but getting it up to 80 degrees will require some work on my home made oven > can i cure at 70 degrees? if so do i just extend the oven time to say 11hours??

ta
Lee.
Reply
Toffee
Toffee
Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)Supreme Being (270 reputation)
Group: Forum Members
Posts: 36, Visits: 118
cheers for the posts and advice guys, some great info here.




My oven is simply 100mm thick 8'x4' celotex insulation board, making my over 2200mm x 2200mm x 1200mm, I have a fan assisted oven internal sas the heater and a very similar control system as shown on the pre preg video that easy composite show on there tutorial.