Hey guys,

New to the composite industry, and have just successfully completed our first mould (Phew).
Was just wondering what is the best way to remove excess filleting wax that is left over on the mould? Tried scraping it off, and using just a regular microfibre cloth, or my finger. Majority of it has been removed however there are still some areas that have it smeared.

Thanks in advance,
JD
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
better test it on a small part of the mould first, didnt ever affect anything on my gelcoat Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search