How to create a resin for prepreg ?


Author
Message
Julien
Julien
Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)
Group: Forum Members
Posts: 16, Visits: 2.8K
I was wondering if there is a way to create a resin to drop on a tissue to obtain a material whose appearance is similar to industrial prepreg, that is to say a material whose weaving is not deformed during the layup or very little.




Thanks,
Edited 10 Years Ago by Julien
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
It's the only way when working with dry fabrics. You can use a surface tissue as well. 