Having had a little read around here it seems that infusion is the method of choice.  All of my projects have been a wet lay, perforated release film, breather fabric and vac bag style lay up.  Its always been good for me so I'd be interested in hearing about the pros and cons of various methods.  Pre-preg is a little out of my reach with no oven or autoclave I'm afraid!
Reply
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I see the point on pin holes, and with the stress free set-up.  How does the technical difficulty fare when compared with wet-lay up?