Here are a few before and after images of a repair i carried out on a BMW hugger.









http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Edited 10 Years Ago by carbonfibreworks
Reply
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
did you do a local repair patch to match the weave or did you do an all over ply? looks a good repair