carbonfibreworks
carbonfibreworks
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
I repaired all the damage first then covered the guard down to the ridge so about 70% ,then a few coats of epoxy resin and after sanding back I sprayed it with 2k clear.
Chris
Carbon fibre works LTD
Reply
Like
7
scottracing
scottracing
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
did you do a local repair patch to match the weave or did you do an all over ply? looks a good repair
Reply
Like
6
Brian_s
Brian_s
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 99,
Visits: 2.5K
Looks good. Well done.
Reply
Like
6
carbonfibreworks
carbonfibreworks
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
Here are a few before and after images of a repair i carried out on a BMW hugger.
Edited
11 Years Ago by
carbonfibreworks
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search