By carbonfibreworks - 1/1/2015 6:28:54 PM
Here are a few before and after images of a repair i carried out on a BMW hugger.
|
By carbonfibreworks - 1/2/2015 9:25:13 AM
I repaired all the damage first then covered the guard down to the ridge so about 70% ,then a few coats of epoxy resin and after sanding back I sprayed it with 2k clear.Chris Carbon fibre works LTD
|
|