I have today mixed and poured my first mould. Whilst degassing small (100 gram) mixes the rubber certainly bubbled up but I did not notice any significant 'collapse' as shown on your tutorial video, even after approximately 5 minutes.

The degassing chamber negative pressure was in excess of 0.8 bar. I left the pump running and chamber outlet valve open during this period.

Any reason I did not notice a collapse and is that negative pressure ok?

Regards

Ray
Replies
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
Sorry, I don't think -0.8 bar is enough. It should be a lot closer to -1 bar.

Brian.
Ray Rogers
Ray Rogers
Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)Supreme Being (150 reputation)
Group: Forum Members
Posts: 18, Visits: 79
Thank you Brian
I thought that and will look into why I am not achieving it.
Regards
Paul (Staff)
Paul (Staff)
Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)Technical Support (1.4K reputation)
Group: Administrators
Posts: 134, Visits: 614
Hi Ray,

Brian is right, at -0.8bar you won't quite reach the point where the entraped air does an 'exponential expansion' the closer you get to absolute vacuum the better. -0.8bar will still help to degass... you would just have to wait much longer for the air to rise and burst in a slightly more 'natural' way. If you have any questions on how to get the most out of your equipment/setup just let me know.

Paul Statham
Easy Composites / Carbon Mods - Technical
sally barratt
sally barratt
Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)
Group: Forum Members
Posts: 1, Visits: 6
Hi,
I have just started using a degasser for casting small models and I do not see the exponential expansion' that every demo seems to have even though I am taking it to the correct vacuum, is it always the case that you will have this happening or do smaller quantities of silicone or resin just not behave in the same way. Also is it the case that you must leave the pump running until this is achieved?