Group: Forum Members
Posts: 18,
Visits: 79
|
I have today mixed and poured my first mould. Whilst degassing small (100 gram) mixes the rubber certainly bubbled up but I did not notice any significant 'collapse' as shown on your tutorial video, even after approximately 5 minutes.
The degassing chamber negative pressure was in excess of 0.8 bar. I left the pump running and chamber outlet valve open during this period.
Any reason I did not notice a collapse and is that negative pressure ok?
Regards
Ray
|