Just decided to have a specific fuel tank mould as knife and forking one from the monocoque mould was never going to be perfect....


Just started laying today too.. so fingers crossed it will be laid up tomorrow...
cured for Wednesday....


Tags
Reply
morepower
morepower
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
Before bonding the two parts are dry fitted to make sure it has an overlap but does not spread the tank open more than the original 

http://www.talkcomposites.com/Uploads/Images/9d758c27-812f-4c21-838d-2afe.jpg

The tank is now bonded and you can see the finished weight.. The original one was 4.5KG
http://www.talkcomposites.com/Uploads/Images/4c8a2b15-8e42-491d-8139-545a.jpg