Hi all,
the aim of this work is to obtain a light, confortable and cool kiteboard  Tongue
Instead of use an usual PU or  wood core I tryed to generate something similar to honeycomb.
At first it needs a lot of meters of carbon's tube.. so you have a roll a lot..
For the top and bottom sheet I chose the carbonkevlar for its elongations properties.

I show you some picture and a quick video with the building process.

For the video:  https://www.youtube.com/watch?v=XEiZ1XdNf-c

Some photo

http://i59.servimg.com/u/f59/13/17/52/45/l_holl10.jpg

http://i59.servimg.com/u/f59/13/17/52/45/l_holl12.jpg

http://i59.servimg.com/u/f59/13/17/52/45/l_holl13.jpg

http://i59.servimg.com/u/f59/13/17/52/45/l_holl14.jpg

http://i59.servimg.com/u/f59/13/17/52/45/l_holl15.jpg

http://i59.servimg.com/u/f59/13/17/52/45/l_holl16.jpg

http://i59.servimg.com/u/f59/13/17/52/45/l_holl17.jpg

http://i59.servimg.com/u/f59/13/17/52/45/l_holl18.jpg

Bye





My You Tube Channel
Edited 11 Years Ago by Brucecreations
Reply
Chris Scott
Chris Scott
Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)
Group: Forum Members
Posts: 20, Visits: 235
At first I didn't realize what the core was! That's gotta be the coolest use for carbon fiber tube I have seen so far.  So nasty! 