By Brucecreations - 11/16/2014 2:03:29 PM				
            
                      
            Hi all, the aim of this work is to obtain a light, confortable and cool kiteboard    Instead of use an usual PU or  wood core I tryed to generate something similar to honeycomb. At first it needs a lot of meters of carbon's tube.. so you have a roll a lot.. For the top and bottom sheet I chose the carbonkevlar for its elongations properties.
  I show you some picture and a quick video with the building process.
  For the video:  https://www.youtube.com/watch?v=XEiZ1XdNf-c
  Some photo
 
  
 
  
 
  
 
  
 
  
 
  
 
  
 
  
  Bye
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Chris Scott - 10/24/2015 5:59:35 PM				
            
                      
            At first I didn't realize what the core was! That's gotta be the coolest use for carbon fiber tube I have seen so far.  So nasty! 
           
		 | 			
		 
	
	
						
		 	
		
	 |