Hi all,
the aim of this work is to obtain a light, confortable and cool kiteboard  Tongue
Instead of use an usual PU or  wood core I tryed to generate something similar to honeycomb.
At first it needs a lot of meters of carbon's tube.. so you have a roll a lot..
For the top and bottom sheet I chose the carbonkevlar for its elongations properties.

I show you some picture and a quick video with the building process.

For the video:  https://www.youtube.com/watch?v=XEiZ1XdNf-c

Some photo

http://i59.servimg.com/u/f59/13/17/52/45/l_holl10.jpg

http://i59.servimg.com/u/f59/13/17/52/45/l_holl12.jpg

http://i59.servimg.com/u/f59/13/17/52/45/l_holl13.jpg

http://i59.servimg.com/u/f59/13/17/52/45/l_holl14.jpg

http://i59.servimg.com/u/f59/13/17/52/45/l_holl15.jpg

http://i59.servimg.com/u/f59/13/17/52/45/l_holl16.jpg

http://i59.servimg.com/u/f59/13/17/52/45/l_holl17.jpg

http://i59.servimg.com/u/f59/13/17/52/45/l_holl18.jpg

Bye





My You Tube Channel
Edited 12 Years Ago by Brucecreations
Zorongo
Zorongo
Supreme Being (402 reputation)Supreme Being (402 reputation)Supreme Being (402 reputation)Supreme Being (402 reputation)Supreme Being (402 reputation)Supreme Being (402 reputation)Supreme Being (402 reputation)Supreme Being (402 reputation)Supreme Being (402 reputation)
Group: Forum Members
Posts: 40, Visits: 330
Beautiful job !

What did you use for the rails / edges ? On the bow and tail it seems you used filler, is it right ? What about the rails ?

Thanks in advance !
Brucecreations
Brucecreations
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 25, Visits: 371
What did you use for the rails / edges ?

I used epoxy resin charged with milled carbon fiber
On the bow and tail it seems you used filler

No, there are two small pieces of balsa wood. When laminated they given to the tails a right amount of rigidity.







My You Tube Channel
Zorongo
Zorongo
Supreme Being (402 reputation)Supreme Being (402 reputation)Supreme Being (402 reputation)Supreme Being (402 reputation)Supreme Being (402 reputation)Supreme Being (402 reputation)Supreme Being (402 reputation)Supreme Being (402 reputation)Supreme Being (402 reputation)
Group: Forum Members
Posts: 40, Visits: 330
Thanks ! Wink
Warren (Staff)
Warren (Staff)
Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)Supreme Being (33K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Looks awesome!

The core must have taken hours to get perfectly right!

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Brucecreations
Brucecreations
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 25, Visits: 371
Thanks, for sure isn't a quik work, you must believe in it Smile





My You Tube Channel
Chris Scott
Chris Scott
Supreme Being (252 reputation)Supreme Being (252 reputation)Supreme Being (252 reputation)Supreme Being (252 reputation)Supreme Being (252 reputation)Supreme Being (252 reputation)Supreme Being (252 reputation)Supreme Being (252 reputation)Supreme Being (252 reputation)
Group: Forum Members
Posts: 20, Visits: 235
At first I didn't realize what the core was! That's gotta be the coolest use for carbon fiber tube I have seen so far.  So nasty! 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search