Hydrofoil kiteboard


Author
Message
Brucecreations
Brucecreations
Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)
Group: Forum Members
Posts: 25, Visits: 371

Hi all. I’d like to show you my lasts work about composites.

I’m  very found in Hydrofoil kiteboarding, so in the past 10 years I do some models Smile

This is the last one. The idea was to build something different  from the models on the market, an hydrofoil easy, stable, and possibly fast.

 Some pictures:

http://www.talkcomposites.com/Uploads/Images/27d687b5-2fad-4669-b885-d01b.jpg

http://www.talkcomposites.com/Uploads/Images/0a443216-d838-4d8e-abae-9b4d.jpg

http://www.talkcomposites.com/Uploads/Images/b0a055ee-411b-4900-87d5-6c7f.jpg

http://www.talkcomposites.com/Uploads/Images/a523129d-6af4-4588-ac41-e60f.JPG

http://www.talkcomposites.com/Uploads/Images/8fd55d0f-c812-4618-94ec-a2a8.jpg

http://www.talkcomposites.com/Uploads/Images/58ad087f-3cbf-463a-9489-ba58.jpg

http://www.talkcomposites.com/Uploads/Images/cfae7f93-d389-4376-9a24-0159.jpg

In this video you can see the first trials.

https://www.youtube.com/watch?v=hP4AcEQYi5w


In this one the building process for the board.

https://www.youtube.com/watch?v=iWn100jdyY0


An old version

http://www.talkcomposites.com/Uploads/Images/5d431796-e2a7-412f-8807-bbcd.jpg

http://www.talkcomposites.com/Uploads/Images/e6d00393-7aa6-4c74-bb8e-004d.JPG


I hope you like

At this moment a new one is growing Wink











My You Tube Channel
Edited 11 Years Ago by Brucecreations
Reply
d21d3q
d21d3q
Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)
Group: Forum Members
Posts: 5, Visits: 22
Brucecreations (01/09/2015)
It's a little bit empirical,
in other experiences, I noted how many layers (and their weight/m2) I used and the thickness reached for planar objects.

Did you think about making wing from two separates parts 


It's what I do

and then glueing them together?

In my opinion isn't enough, You have to join also with a fabrics.


I am a little bit confused - here you are opening mould with wing and right before you were presenting stack of prepared layers of different size. This suggest that it was made in single process. i guess that it requires specific amount of material to be put inside.
Making it from two separate parts (infusion?) would require such precise dosing of material. (wing form two halves might be hollow inside?)

It's full carbon, various pattern and some Hight moulus.

You mean full like this

or more like this

but fully hollow?

Lawrence (02/09/2015)
HI All,

I'm thinking to use modeling clay to make a mold.My idea is to when clay is harden and then apply chopped strand mat.I wonder if this is a feasible method?

Lawrence

Here some guy is describing how he uses clay to produce molds.


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Brucecreations - 11 Years Ago
wozza - 11 Years Ago
Brian2fast - 11 Years Ago
ChrisR - 11 Years Ago
Brucecreations - 11 Years Ago
Brucecreations - 11 Years Ago
kidpaint - 11 Years Ago
Brucecreations - 10 Years Ago
kidpaint - 10 Years Ago
Brucecreations - 10 Years Ago
davro - 10 Years Ago
Dravis - 10 Years Ago
tomzi1234 - 10 Years Ago
Brucecreations - 10 Years Ago
Hanaldo - 10 Years Ago
Brucecreations - 10 Years Ago
Hanaldo - 10 Years Ago
davro - 10 Years Ago
Jacopo Carbonio - 10 Years Ago
Dravis - 10 Years Ago
carbonfibreworks - 10 Years Ago
Brucecreations - 10 Years Ago
Dravis - 10 Years Ago
Brucecreations - 10 Years Ago
tomzi1234 - 10 Years Ago
Brucecreations - 10 Years Ago
Hanaldo - 10 Years Ago
Brucecreations - 10 Years Ago
d21d3q - 10 Years Ago
Brucecreations - 10 Years Ago
d21d3q - 10 Years Ago
Lawrence - 10 Years Ago
Brucecreations - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search