Hi all. I’d like to show you my lasts work about composites.

I’m  very found in Hydrofoil kiteboarding, so in the past 10 years I do some models Smile

This is the last one. The idea was to build something different  from the models on the market, an hydrofoil easy, stable, and possibly fast.

 Some pictures:

http://www.talkcomposites.com/Uploads/Images/27d687b5-2fad-4669-b885-d01b.jpg

http://www.talkcomposites.com/Uploads/Images/0a443216-d838-4d8e-abae-9b4d.jpg

http://www.talkcomposites.com/Uploads/Images/b0a055ee-411b-4900-87d5-6c7f.jpg

http://www.talkcomposites.com/Uploads/Images/a523129d-6af4-4588-ac41-e60f.JPG

http://www.talkcomposites.com/Uploads/Images/8fd55d0f-c812-4618-94ec-a2a8.jpg

http://www.talkcomposites.com/Uploads/Images/58ad087f-3cbf-463a-9489-ba58.jpg

http://www.talkcomposites.com/Uploads/Images/cfae7f93-d389-4376-9a24-0159.jpg

In this video you can see the first trials.

https://www.youtube.com/watch?v=hP4AcEQYi5w


In this one the building process for the board.

https://www.youtube.com/watch?v=iWn100jdyY0


An old version

http://www.talkcomposites.com/Uploads/Images/5d431796-e2a7-412f-8807-bbcd.jpg

http://www.talkcomposites.com/Uploads/Images/e6d00393-7aa6-4c74-bb8e-004d.JPG


I hope you like

At this moment a new one is growing Wink











My You Tube Channel
Edited 11 Years Ago by Brucecreations
Replies
Brucecreations
Brucecreations
Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)Supreme Being (264 reputation)
Group: Forum Members
Posts: 25, Visits: 371
That is freakin massive spread tow carbon haha


I love the spread tow, I started with the 15 mm, but it wasn't enough, I used the 25 mm (changing the pattern from plain to twill....Doze) but I needed something more...

This one is 90 mm.... I think could be eonough..... for the moment.BigGrin  








My You Tube Channel
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Brucecreations (25/06/2015)
That is freakin massive spread tow carbon haha


I love the spread tow, I started with the 15 mm, but it wasn't enough, I used the 25 mm (changing the pattern from plain to twill....Doze) but I needed something more...

This one is 90 mm.... I think could be eonough..... for the moment.BigGrin  




I'm a big fan of spread tow, very unique fabric. Bit of a pain to work with, but it's worth it for the looks. Had no idea you could even get a 90mm, it's outrageous haha. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Brucecreations - 11 Years Ago
wozza - 11 Years Ago
Brian2fast - 11 Years Ago
ChrisR - 11 Years Ago
Brucecreations - 11 Years Ago
Brucecreations - 11 Years Ago
kidpaint - 11 Years Ago
Brucecreations - 10 Years Ago
kidpaint - 10 Years Ago
Brucecreations - 10 Years Ago
davro - 10 Years Ago
Dravis - 10 Years Ago
tomzi1234 - 10 Years Ago
Brucecreations - 10 Years Ago
Hanaldo - 10 Years Ago
Brucecreations - 10 Years Ago
Hanaldo - 10 Years Ago
davro - 10 Years Ago
Jacopo Carbonio - 10 Years Ago
Dravis - 10 Years Ago
carbonfibreworks - 10 Years Ago
Brucecreations - 10 Years Ago
Dravis - 10 Years Ago
Brucecreations - 10 Years Ago
tomzi1234 - 10 Years Ago
Brucecreations - 10 Years Ago
Hanaldo - 10 Years Ago
Brucecreations - 10 Years Ago
d21d3q - 10 Years Ago
Brucecreations - 10 Years Ago
d21d3q - 10 Years Ago
Lawrence - 10 Years Ago
Brucecreations - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search