Hi, I want to start making parts using Carbon and Kevlar. Initial requirement is for a duct. I am contemplating a 3D printed investment mould using ABS or PLA. I have seen it is possible but cannot find any videos showing the process.

The parts will not be massive, perhaps 500mm cube. I would like to be able to start on a relatively low budget so anyone with existing facilities who would be able to help out in the locality I would appreciate it.

Charlie
Replies
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Where abouts are you ? got a fair amount of kit inc vac pumps/small oven an can get access to several claves or point you in the right direction

Im between wymondham an Norwich

rob
fusionfanatic
fusionfanatic
Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)
Group: Forum Members
Posts: 6, Visits: 23
f1rob (07/11/2014)
Where abouts are you ? got a fair amount of kit inc vac pumps/small oven an can get access to several claves or point you in the right direction

Im between wymondham an Norwich

rob


That's great, I have sent a pm
fusionfanatic
fusionfanatic
Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)
Group: Forum Members
Posts: 6, Visits: 23
f1rob (07/11/2014)
Where abouts are you ? got a fair amount of kit inc vac pumps/small oven an can get access to several claves or point you in the right direction

Im between wymondham an Norwich

rob


That's great, I have sent a pm
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
fusionfanatic - 11 Years Ago
wozza - 11 Years Ago
fusionfanatic - 11 Years Ago
                 why do you think you need an autoclave?
ChrisR - 11 Years Ago
fusionfanatic - 11 Years Ago
wozza - 11 Years Ago
ChrisR - 11 Years Ago
                                 [quote][b]ChrisR (07/11/2014)[/b][hr]Yes, I was a little rushed earlier to expand on my original...
fusionfanatic - 11 Years Ago
f1rob - 11 Years Ago
fusionfanatic - 11 Years Ago
fusionfanatic - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search