By fusionfanatic - 11/6/2014 11:58:59 PM

Hi, I want to start making parts using Carbon and Kevlar. Initial requirement is for a duct. I am contemplating a 3D printed investment mould using ABS or PLA. I have seen it is possible but cannot find any videos showing the process.

The parts will not be massive, perhaps 500mm cube. I would like to be able to start on a relatively low budget so anyone with existing facilities who would be able to help out in the locality I would appreciate it.

Charlie
By fusionfanatic - 11/8/2014 4:51:46 PM

f1rob (07/11/2014)
Where abouts are you ? got a fair amount of kit inc vac pumps/small oven an can get access to several claves or point you in the right direction

Im between wymondham an Norwich

rob


That's great, I have sent a pm