Hi all.  I have inherited a 6ft long wooden model boat built in the late 1940's that I am attempting to bring back to life.  The wooden planked hull is sound but was covered in canvas that is rotten and I believe epoxy resin would provide a modern waterproofing solution.
Questions / recommendations:  would a epoxy coating resin suffice or would it be better to use a glass surface tissue or a filler powder ( microballons ) for durability ?    Is it possible to add a pigment or is it preferable to paint the resin later - to keep the boat original it needs to be sand coloured.
Any advice greatly appreciated as boat too precious to make a mess of it. 
Cheers.
Roger.
Reply
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
Nice, get some photos up... I've got a half built 3ft fire tender I've been building for 20+ years