By Roger Frank - 11/3/2014 4:52:34 PM
Hi all. I have inherited a 6ft long wooden model boat built in the late 1940's that I am attempting to bring back to life. The wooden planked hull is sound but was covered in canvas that is rotten and I believe epoxy resin would provide a modern waterproofing solution. Questions / recommendations: would a epoxy coating resin suffice or would it be better to use a glass surface tissue or a filler powder ( microballons ) for durability ? Is it possible to add a pigment or is it preferable to paint the resin later - to keep the boat original it needs to be sand coloured. Any advice greatly appreciated as boat too precious to make a mess of it. Cheers. Roger.
|
By ChrisR - 11/4/2014 7:49:20 AM
Nice, get some photos up... I've got a half built 3ft fire tender I've been building for 20+ years
|
|