Hello,

I'm making my airbox for my bike. I did the mould but I don't know quite right which technique to apply for the airbox making: the infusion or the bagging.
What can you advise me for my project?

Here my mould:http://www.talkcomposites.com/Uploads/Images/6aa8bc9c-96ca-4790-86fd-7265.JPG

http://www.talkcomposites.com/Uploads/Images/9bf9be3a-86ba-4338-882f-26b7.JPG


http://www.talkcomposites.com/Uploads/Images/4be89538-df0f-443d-9b6f-2a06.JPG


http://www.talkcomposites.com/Uploads/Images/9b99e86b-f001-4e2c-b674-d52c.JPG


Thanks in advance
Reply
20_rc51_00
20_rc51_00
Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)
Group: Forum Members
Posts: 95, Visits: 548
infusion can be done but i personally have learned to hate it since all the dry fabric is a pain to handle and get into the contours. The best way for such an intricate part as that would be prepreg since you can cut pieces to fit perfectly into the curvatures and then easily massage them into the corners. If I was working with that mold I would try some sort of in mold coating so that you have some good tacky base to lay the dry fibers onto. There appears to be no flanges on your molds so it makes infusion very tricky. 