Test core material infusion


Author
Message
pahanes
pahanes
Supreme Being (297 reputation)Supreme Being (297 reputation)Supreme Being (297 reputation)Supreme Being (297 reputation)Supreme Being (297 reputation)Supreme Being (297 reputation)Supreme Being (297 reputation)Supreme Being (297 reputation)Supreme Being (297 reputation)
Group: Forum Members
Posts: 29, Visits: 20K
1 core layer Lantor SoricXF 3mm. Left 1 layer carbon cloth and right 2 layers on the front side.
Concluded: to lay down 2-3 layers of carbon fiber on the front side in order to avoid the impression.
p.s. weight plates 20x20 cm = 100 grams )  Lightweight and durable )
Infusion without mesh, without peel-ply.



Edited 11 Years Ago by pahanes
Reply
pahanes
pahanes
Supreme Being (297 reputation)Supreme Being (297 reputation)Supreme Being (297 reputation)Supreme Being (297 reputation)Supreme Being (297 reputation)Supreme Being (297 reputation)Supreme Being (297 reputation)Supreme Being (297 reputation)Supreme Being (297 reputation)
Group: Forum Members
Posts: 29, Visits: 20K
wozza (02/10/2014)
As I don't know the reason for the test this may be an unfair comment but for a core to add any real strength it needs to have balanced layers of reinforcement either side of it, hence the term core. When there is only reinforcement on one side the stack can delaminate under load.

Warren


Reason for the test - to see whether leaves imprint Soric XF
Edited 11 Years Ago by pahanes
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search