Talk Composites - The Forum for Advanced Composites

Test core material infusion

http://www.talkcomposites.com/Topic13123.aspx

By pahanes - 10/2/2014 1:47:49 PM

1 core layer Lantor SoricXF 3mm. Left 1 layer carbon cloth and right 2 layers on the front side.
Concluded: to lay down 2-3 layers of carbon fiber on the front side in order to avoid the impression.
p.s. weight plates 20x20 cm = 100 grams )  Lightweight and durable )
Infusion without mesh, without peel-ply.


By pahanes - 10/2/2014 4:52:42 PM

Ok. I do the same on both sides Smile