Just made some wall panels for a shower enclosure (refused to pay £150 a panel plus fitting kitWink )

I have a 2.1m x 1.2m double glazed unit that I use for infusing flat sheet.

Sprayed down some white gelcoat, once tacked off I layed down one layer of resin rich 450grm CSM. Whilst still wet I placed a 2m x 1m sheet of 9mm MDF (scored the face with a Stanley knife to aid bonding) onto the wet CSM and weighted it down.

Once cured the sheet was demoulded and cut to size. Result one mirror finish wall panel.





Cost : materials £50 plus two hours labour.Smile

Warren

Carbon Copies Ltd
Reply
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
I job I started and havnt finished yet for the home is a spread tow carbon splash back for behind the cooker/hob in our kitchen. Made the sheet, just havnt got round to actually cutting it to shape and putting it on the wall!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
wozza - 11 Years Ago
ChrisR - 11 Years Ago
wozza - 11 Years Ago
Warren (Staff) - 11 Years Ago
ChrisR - 11 Years Ago
brainfart - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Jonas - 11 Years Ago
Dravis - 11 Years Ago
FLD - 11 Years Ago
ajb100 - 11 Years Ago
wozza - 11 Years Ago
Dravis - 11 Years Ago
wozza - 11 Years Ago
Warren (Staff) - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
kidpaint - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search