I'm looking for a carbon fibre material upon which to sit materials to be furnaced; what is the maximum working temperature of the carbon fibre sheet or fabric materials?


The process currently operates between 900 and 1000 C for several hours, will any of the materials be able to withstand these conditions?
Reply
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Never seen a data sheet for it but depending on race/exhaustcoatings an design the panels are seeing 1000-1100 deg for most of a 2hr ish race distance