So I have a rather simple part with one area that I thought was going to be simple, but is causing a lot of issues.  I could use some advice as to how to lay the fiber in so I don't have the issues with bunching that I can't seem to get around.

The part can be made like this easily but obviously it will not be optimal visually.
Attachments
IMG_20140819_103038_899.jpg (516 views, 528.00 KB)
IMG_20140819_104536_161.jpg (428 views, 486.00 KB)
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
This part is not at all simple! I find it amazing how well the twill weave conforms to the surface, but I think that even if you used satin weave you still couldn't do it without some cuts and overlapping.
Edited 11 Years Ago by brainfart
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
With those sharp edges I'd have thought it would be easier to make the surface layer in pro-finish and do it in several pieces.  If you make the corners the join line it wont be easy to spot.
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
anyone can show images how to overlap that>?