Group: Forum Members
Posts: 592,
Visits: 1.9K
|
Sounds like your Vac-bag-film is not the best quality, or has been poorly stored in a "prickly" environment -- minute glass-fibre fragments and CF fragments can puncture some bagging film (EC's elastic film is not very good in this respect, I'm sorry to say)
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
|