So I've been trying to make some parts using vacuum infusion. I have bagged 6 parts now and have only infused 3 of them. On two of the parts the bag failed and ruined the parts. The other three are still in the mold under a vacuum bag that I cannot get the leaks out of. I don't know why I'm having so many problems with this. I even bought a sonic tester to listen for the smallest of leaks and can't find any, but yet every time I do a drop test I get a 1" drop in pressure for every 20-30 minutes. I've gone over and over these parts. I've even re-bagged them!!! I'm almost at my wits end here! I feel like I've actually become pretty good at the bagging process other than being unable to stop all of the leaks. Can anyone give me any advice?
Oh, I also have completely coated all sides of the molds because I thought that my leak was possibly going through the part. Yet that had no effect...
|