Hi folks,

I've posed this question in the mould making section a few days ago but I'm looking for a more definitive answer from you guys.

I've been using the above on my current project (model aircraft) and have been impressed with it's hardness when cured. But I find it's quite thick to brush on and doesn't flow very well, leaving quite an irregular surface .  Is it possible to thin it slightly so that it flattens out better?

Many thanks, Marty

Reply
Warren (Staff)
Warren (Staff)
Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)Supreme Being (25K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
ChrisR is right, The Epoxy Tooling Gelcoat is deliberately viscous.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search